학술논문

Ferroelectricity of Hf0.5Zr0.5O2 Thin Film Induced at 350°C by Thermally Accelerated Nucleation During Atomic Layer Deposition
Document Type
Periodical
Source
IEEE Transactions on Electron Devices IEEE Trans. Electron Devices Electron Devices, IEEE Transactions on. 71(4):2690-2695 Apr, 2024
Subject
Components, Circuits, Devices and Systems
Engineered Materials, Dielectrics and Plasmas
Temperature measurement
Electrodes
Crystallization
Capacitors
Annealing
Tin
Plasma temperature
Atomic layer deposition (ALD)
ferroelectric
Hf₀.₅Zr₀.₅O₂ (HZO)
low thermal budget thin film
Language
ISSN
0018-9383
1557-9646
Abstract
(Hf,Zr) $\text{O}_{{2}}$ -based ferroelectric thin films have recently received significant interest as next-generation memory device materials. However, the high crystallization temperature of over 500 °C to obtain robust ferroelectricity entails challenges for integrating (Hf,Zr) $\text{O}_{{2}}$ -based ferroelectrics in back-end-of-line (BEOL) processing, which requires temperatures less than 400 °C. In this study, we suggest an effective yet simple method to reduce the crystallization temperature by thermally accelerating the nucleation on 10-nm-thick Hf $_{{0.5}}$ Zr0.5O2 (HZO) film during atomic layer deposition (ALD). Increasing the deposition temperature facilitated seed nuclei of tetragonal/orthorhombic phases, which in turn reduced the crystallization temperature as well as augmented the formation of the ferroelectric orthorhombic phase. Consequently, the HZO film grown at an ALD deposition temperature of 300 °C exhibited switchable polarization (2Pr) of $26.9~\mu \text{C}$ /cm2 and endurance up to $10^{{8}}$ cycles after rapid thermal processing (RTP) at 350 °C. This work elucidates that forming seed nuclei of tetragonal/orthorhombic phases by increasing the deposition temperature can be a promising strategy to fabricate the BEOL-compatible HZO thin films.