Effect of severe plastic deformation on the biocompatibility and corrosion rate of pure magnesium.
Document Type
Article
Source
Journal of Materials Science. May2017, Vol. 52 Issue 10, p5992-6003. 12p. 1 Color Photograph, 2 Diagrams, 1 Chart, 5 Graphs.
Subject
*MATERIAL plasticity
*BIOCOMPATIBILITY
*CORROSION & anti-corrosives
*MAGNESIUM alloys
*MECHANICAL behavior of materials
Language
ISSN
0022-2461
Abstract
It is well established that magnesium has a considerable potential for use as a biodegradable material. This report describes the effect of processing by severe plastic deformation (SPD) on the grain refinement, mechanical behavior, biocompatibility and corrosion behavior of commercial purity magnesium. The material was received as cast slabs and processed by rolling, equal-channel angular pressing and high-pressure torsion to produce samples with average grain sizes in the range of ~0.5-300 μm. The results show that severe plastic deformation does not affect the biocompatibility. However, the corrosion behavior is affected by the processing route. Specifically, SPD processing leads to general corrosion as opposed to localized corrosion in the as-cast and hot-rolled condition. [ABSTRACT FROM AUTHOR]