PUREX style jumper connector type III gasket test report
Document Type
Technical Report
Author
Source
Other Information: PBD: Jul 1993
Subject
12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE WASTES FROM NUCLEAR FACILITIES GASKETS
PERFORMANCE TESTING
PUREX PROCESS
TEFLON
HANFORD RESERVATION
VITRIFICATION
RADIOACTIVE WASTE FACILITIES
WASTE PROCESSING PLANTS
DEFORMATION
MECHANICAL PROPERTIES
RADIOACTIVE WASTE PROCESSING 052001
WASTE PROCESSING
Language
English
Abstract
This report summarizes data obtained from testing of type III Teflon gaskets used on PUREX-type process jumper connectors. The purpose of these tests was to asses the performance characteristics of the type III gaskets, currently planned to be used in the Hanford Waste Vitrification Plant (HWVP). Results indicate that the Teflon gaskets deform severally under heat and applied moment loads. The gaskets also lose their ability to hold pressure when thermally cycled, and cannot hold elevated pressures unless they are retorqued between cycles. Gasket failure ultimately occurs after one or more cycles.