학술논문

발수코팅된 커피박을 혼입한 벽돌용 모르타르의 압축강도 및 흡수율
Compressive Strength and Absorption Ratio of Mortar for Brick Incorporating Spent Coffee Grounds Coated with Water Repellent
Document Type
Article
Source
대한건축학회논문집, 39(5), 415, pp.189-196 May, 2023
Subject
건축공학
Language
한국어
ISSN
2733-6247
2733-6239
Abstract
Recently, as the amount of coffee consumption increases, the amount of spent coffee grounds increases, but the amount recycled is small andutilization in the construction field is insufficient. Therefore, in this study, the properties of mortar and the quality of bricks were evaluatedby replacing a part of the amount of cement used with spent coffee grounds coated with a water repellent. As a result, the mortarincorporating the spent coffee grounds coated with the water repellent improved the compressive strength, density and absorption ratiocompared to the mortar incorporating the spent coffee grounds not coated with the water repellent. In addition, the quality of the bricksmanufactured based on the appropriate replacement ratio of the water repellent coated spent coffee grounds satisfied all KS standards. Therefore, it is considered that the appropriate W/B for manufacturing bricks is 38%, and the appropriate replacement ratio of water repellentcoated spent coffee grounds is up to 6%.
커피소비량이 증가함에 따라 커피박 발생량이 증가되지만 재활용되는 양은 적으며 건설분야에서도 활용이 미비하다. 따라서 본 연구에서는 시멘트 사용량의 일부를 발수제로 코팅된 커피찌꺼기로 치환한 모르타르의 물성과 벽돌의 품질을 평가하였다. 그 결과, 발수제로 코팅된 커피박을 혼입한 모르타르가 발수제로 코팅시키지 않은 커피박을 혼입한 모르타르 대비 압축강도, 밀도 및 흡수율이 향상되었다. 또한, 발수코팅된 커피박의 적정 치환율을 기반으로 제작한 벽돌의 품질은 KS 기준을 모두 충족하였다. 따라서, 벽돌의 제작을 위한 적정 W/B는 38%, 발수코팅된 커피박의 적정 치환율은 6%까지라고 사료된다.